摘 要:介紹煤棒制作的工藝和要求,即原料煤粉含水質(zhì)量分?jǐn)?shù)<8%,配制后原料含水質(zhì)量分?jǐn)?shù)<13%,漚化時(shí)間一般為24 h,烘干后煤棒含水質(zhì)量分?jǐn)?shù)<4%。以煤棒制氣時(shí),應(yīng)適當(dāng)提高入爐蒸汽壓力和汽量,爐上溫度一般控制在(280±20)℃,爐下溫度一般控制在(300±20)℃,并應(yīng)調(diào)整吹風(fēng)百分比,增加下灰次數(shù)。采用煤棒制氣,可充分利用碎煤、粉煤,噸氨成本下降140元,噸尿素成本下降90元以上,經(jīng)濟(jì)效益顯著。
關(guān)鍵詞:煤棒;制氣;總結(jié)
Sum-Up of Use of Coal Rod for Gasification
Yao Liexia,Jing Wenge
(Shanxi Yongji Zhongnong Chemical Co.,Ltd. 044500)
Abstract:The process and requirements are given for the manufacture of coal rods,viz.,feed coal powder with a water content of <8% mass fraction,water content of feed afte....